Moisture content

Moisture content is the amount of water present in a material, expressed as a percentage of its weight, which for many plastics must be very low before processing.

What it means

Hygroscopic plastics take in water from humid air, and the monsoon makes this worse. Even a small amount can spoil a moulded part. Moisture content is checked with a moisture analyser, and the resin supplier states the maximum allowed before processing. The same term is used for raw materials like wood, paper and grain, where excess moisture affects weight, shelf life and quality.

Example

A moulder gets a lot of PET resin in July. The incoming check reads 0.08 percent moisture, while the processing limit is 0.005 percent. The lot goes to the dryer for 6 hours, is re-tested at 0.004 percent and only then released to the machine, which avoids a day of rejected bottles.

Records and checks

  • Record the material, lot, test method, the measured moisture, the limit and the result with date and time.
  • Verify the analyser against a standard sample on a schedule and re-test after any long storage.
  • Stores test at receipt, the operator tests before moulding, and quality keeps the records and reviews trends.

Common mistakes

  • Leaving open bags on the floor in humid weather and moulding them without testing.
  • Testing at receipt only, and not again after weeks in stock.