Sink mark
A sink mark is a small depression on the surface of a moulded part, usually above a thick section, caused by plastic shrinking as it cools.
What it means
Thick areas cool and shrink last. As the inner plastic contracts, it pulls the skin inward and leaves a dent. Sink marks are usually fixed by increasing the holding pressure or time, lowering the melt temperature or shortening the cooling path. Design changes can help, such as thinner ribs or coring out thick bosses. Appearance parts may be rejected for even faint sinks.
Example
A television bezel shows dents over its screw bosses. The mould designer changes the boss wall to 60 percent of the main wall thickness, and the setter increases the holding time by 3 seconds. After both changes, the dents are gone and the buyer approves the part.
Records and checks
- Record the location and depth of sinks, the process settings in use and the changes tried.
- Verify the parts under good light against a limit sample agreed with the buyer.
- The setter adjusts the process, the tool room advises on design changes, and the quality inspector approves the final sample.
Common mistakes
- Cutting cooling time to save seconds, which can make sinks worse.
- Raising the holding pressure so far that it causes flash and sticking.