Warpage

Warpage is the distortion of a moulded part, such as bending, bowing or twisting, caused by uneven cooling or shrinkage so that it no longer matches its intended shape.

What it means

Plastic shrinks as it cools, and if one area cools or shrinks more than another, the part bends. Common causes are uneven wall thickness, different temperatures on the two mould halves, early ejection, high packing stress and long flow in one direction. Warpage shows up on flat parts like trays, panels and lids, which then fail to fit or seal. Fixes may involve both the process and the design.

Example

A flat tray rises 3 mm at the corners after ejection, while the buyer allows 1 mm. The setter finds the moving half of the mould 15 °C hotter than the fixed half. After balancing the temperatures and adding 4 seconds of cooling, the tray lies within 0.8 mm.

Records and checks

  • Record the amount of warp measured on a gauge or flat surface, with the mould temperatures and cooling time used.
  • Verify parts after cooling for a set time, since some warpage appears only hours after moulding.
  • The setter adjusts, the quality inspector measures, and the tool room reviews the cooling layout if the problem persists.

Common mistakes

  • Checking parts straight off the machine, while still warm, and missing warp that develops later.