Holding pressure

Holding pressure is the pressure applied by the injection screw after the cavity is filled, to pack more plastic in and offset shrinkage while the part cools.

What it means

Plastic shrinks as it cools. If injection stopped at fill, parts would show sink marks and be underweight. Holding pressure, also called packing pressure, keeps pushing plastic into the cavity until the gate freezes. The pressure and its duration set how much material is packed in. Too low gives sinks and voids, too high gives flash, stress and parts that stick in the mould.

Example

A thick-ribbed housing shows sink marks at the rib roots. The process engineer raises the holding pressure from 40 to 55 bar and extends the holding time by 2 seconds. The sinks disappear, and part weight rises from 82.4 g to 83.1 g, which becomes the new weight standard.

Records and checks

  • Record the holding pressure, holding time, the part weight, the machine and the mould for each approved setting.
  • Verify that the part is free of sink marks and flash and that its weight sits within the control limits.
  • The process engineer sets it, the operator keeps to it, and the quality inspector checks weights each hour.

Common mistakes

  • Setting it equal to injection pressure by default instead of finding the right value.
  • Ending the hold before the gate freezes, so plastic flows back out of the cavity.
Did not find your answer?Message the lamp team on WhatsApp. Ask about setup, your records, or anything we have not covered here.Ask us on WhatsApp →