Short shot
A short shot is an incomplete moulded part where the plastic did not fill the whole cavity, leaving a missing corner, edge or section.
What it means
It happens when the melt freezes or runs out before reaching the end of the flow path. Typical causes are low injection pressure or speed, low melt or mould temperature, a blocked gate or vent, too small a shot size or a thin section far from the gate. A short shot is also used on purpose in trials: parts are made with partial fill to see how the plastic flows and whether the cavities fill evenly.
Example
A thin-walled tray comes out with one corner missing on every fifth shot. The setter finds a clogged vent at that corner, where trapped air blocks the flow. After cleaning the vent, the tray fills fully and the missing corner stops, with no change in pressure.
Records and checks
- Record each short shot with the cavity, time, settings in use and the likely cause found.
- Verify the shot size, the cushion and the vents, and check the supply of material in the hopper.
- The operator reports, the setter diagnoses, and the quality inspector sorts out any suspect parts from the lot.
Common mistakes
- Raising injection pressure each time instead of finding a clogged vent or cold spot.
- Letting short shots mix with good parts in the same carton.